Celebration of Clay 2019: Many Hands, Many Ways
Exhibition was held at Santa Fe Clay, Santa Fe, New Mexico from April 26 thru June 5, 2019
JavaScript is not supported
JavaScript required. Your web browser either does not support JavaScript, or it is switched off. Some features may not work properly.
<< All album photos
7/70 photos
< Previous
Next >
Uploaded 08 Jan 2021 |
Judy Nelson-Moore
(Administrator)
Georgia Barnes: BB 3
Cone 10 Supersculpt clay coated with crackly terra sigillata before bisque. Applied a Cobalt Carbonate wash and fired it in a high-fire reduction.; 11.75" x 3.5" x 14"; $300